(A) According to the required SPC sheet thickness, through the upper end of the Mold hollow adjustment screws (M30*2) To adjust the die size, the normal situation of the SPC plate thickness and mold opening size is the same


(B) When the thickness of the SPC sheet is uneven, the same way, by loosening and tighten the top of the mold hollow adjust the screws (M30*2), for the thickness of the sheet, tighten the sheet thinner, loosen the sheet thicker, adjust the thickness of the SPC sheet to the ideal depth, be sure to lock the nut tight.


(C) When the mold stopped working (mould still at high temperature), to immediately remove the mold and clear the mold cavity materials, to avoid the mold by high-temperature materials burned, if you can determine the SPC formula materials are completely extruded by the cleaning materials also no need to disassemble the mould.



(D)When the mold is opened to check whether there is damage, such as burns or mild damage, please use copper slices to eradicate the first clean, and then with 200 mesh grease grinding smooth, and finally apply antirust oil


(E) Strictly prohibit the use of hard material to hit the mould flow path, resulting in damage.